My working notes on 3D printing, kept up to date as I learn. Search everything, switch to one of my printers to see what each tip means on it, and use the infill finder to pick a pattern for the job.

Every fact links to its source, and the page grows as I print more.

  • 17 tips
  • 9 build surfaces
  • 7 specialist filaments
  • 21 infill patterns
  • 14 sources

Start here

The 5 habits that fix most prints. Tap one for the details.

  1. Bake cardboard spools on a 65 °C bed overnight
  2. Jams live at the heatbreak: clear them there
  3. First layer should look glossy and sealed
  4. Tilt right angles 45° to skip supports
  5. Small part? 100% infill

Step-by-step fixes

Repairs written out as steps you can tick off, each with a short clip of just that step.

My printer

Tips

Moisture, clogs and nozzles

Most failures start above the nozzle, or in old, wet plastic.

A hotend cut in half: cold heatsink fins on top, a narrow heatbreak throat, then the heater block and nozzle. The jam point is marked at the heatbreak.coldhotjams here
Jams form where the cold heatsink meets the hot heatbreak throat, not at the nozzle tip.

Bake cardboard spools on a 65 °C bed overnight

On my QIDI Max4 The QIDI Box dries spools too, but give cardboard spools a night on the bed first.

Why and how
Cardboard holds more water than the filament does. Put damp spools on a 65 °C heated bed overnight, then run a normal filament dryer.

[1]

Cloudy, brittle, 2+ years old? Bin it

Why and how
Over about two years, water reacts with the plasticiser and prints turn cloudy, clumpy and glass-brittle. Hydrolysis can’t be undone, so throw the spool out before it crystallises and clogs the nozzle for good.

[1]

Jams live at the heatbreak: clear them there

On my QIDI Max4 For a jam in the gear extruder, follow the step-by-step Max4 clog fix (Step-by-step fixes, above).

Why and how
Skip the acupuncture needles. Unload, snip the end at an angle, open the extruder, poke the heatbreak with a pick, brush out debris and reload. Or raise the temperature 20 to 30 °C and purge.

[1]

Max4 jammed? Follow the step-by-step fix New

Why and how
QIDI’s video for unclogging the gear version of the Max4 extruder, written out as 20 steps you can tick off. Each step has a Show me button that plays just that part, so there’s no pausing and rewinding.

[7]

Ramrod only when nothing else works

Why and how
Heat the nozzle, release the drive tension and push a rounded spring-steel rod down the filament path. Purge 3 to 4 times afterwards. Misused, it can damage gears or the gantry.

[1]

Purge filament between temps, cleaning filament for flecks

On my QIDI Max4 The QIDI Box purges on every colour change. Raise purge volume in QIDI Studio if old colour bleeds in.

Why and how
Use HDPE purge filament between hot and cold plastics (say ASA to PLA) and before nozzle swaps. Use sticky cleaning filament for complex high-flow nozzles that show black flecks or keep underextruding.

[1]

Hardened steel nozzles max out at 260 °C

On my QIDI Max4 The hotend reaches 370 °C, well past the 260 °C limit for hardened steel. Check the nozzle before running hot composites.

On my Ender-3 V3 SE This hotend tops out at 260 °C anyway, so a hardened steel nozzle is safe at every temperature it can reach.

Why and how
Hardened steel loses its temper above 260 °C. High-temperature composites need a tungsten carbide or gemstone-tipped nozzle.

[1]

Fibres grind the nozzle tip shorter

On my Ender-3 V3 SE I suspect glow-in-the-dark PLA wore out a brass nozzle on this printer. Abrasive filaments get a hardened nozzle now.

Why and how
Abrasive fibres file the tip down against the cooled layers below, rather than reaming out the bore. Bigger bore sizes are just the same pointed drill profile, ground shorter.

[1]

First layer and build plates

Glossy and sealed is the target.

Drag the nozzle: glossy, sealed lines mark the right Z offset
A nozzle above a build plate laying four beads of plastic. The beads change shape as the nozzle moves.PEI SPRING STEEL BUILD PLATE

Too high: round beads with gaps between them. Weak adhesion, and wafer-thin lines mean underextrusion.

First layer should look glossy and sealed

On my QIDI Max4 Baby-step Z offset on the screen in 0.05 mm steps during the first layer.

On my Ender-3 V3 SE Baby-step Z offset from Fluidd during the first layer.

Why and how
Tune Z offset live by baby-stepping during the first layer. Even matte filaments should lay down a shiny, fully sealed first layer. The one exception is warp-prone ABS, which likes being squashed a little lower into the adhesive.

[1]

Wait for the plate to cool, then pop it off

On my QIDI Max4 Double-sided textured PEI: let it cool fully before flexing the plate.

Why and how
Wait until the plate is fully cold. Use a plastic razor or scraper, or warm water on glue stick for TPU and PEBA. A wood block only as a last resort.

[1]

Fibre-filled filaments

What fibres really do.

Fibres = stiffer, not stronger

Why and how
Short carbon or glass fibres make prints weaker than the plain plastic. What you get is stiffness, faster solidifying, tighter tolerances and a clean finish, which suits gears, brackets and latches.

[1]

Carbon: conducts. Glass: insulates

Why and how
Heat: carbon conducts it (flatter prints), glass insulates (tougher, easier to anneal). Electricity: carbon is mildly conductive (anti-static, and a weak Faraday cage that drops antenna signal), glass is an insulator.

[1]

Orientation and finishing

Turn the part before you fight supports.

Left: a right-angle bracket printed flat needs support under its overhang. Middle: the same bracket tilted 45 degrees needs no support. Right: a part seen from above with round mouse ears at its four corners.FLAT: NEEDS SUPPORTTILTED 45°: NONEFROM ABOVE: MOUSE EARS
Tilt right angles 45° to drop supports. Anchor sharp corners with mouse ears 10 to 20 mm wide and 3 to 5 layers thick.

Tilt right angles 45° to skip supports

Why and how
Tilting right-angle shapes 45° on the plate removes the need for supports and the stair-stepping that comes with them.

[1]

Thick mouse ears on corners, not thin brims

Why and how
Add 10 to 20 mm mouse ears, 3 to 5 layers thick, at sharp corners. They anchor corners far better than a single-layer brim.

[1]

Zap strings with a blue flame

Why and how
For cobweb-prone filaments like TPU, skip the retraction towers. Toast strings quickly with a blue-flame torch lighter (never a sooty yellow flame) or shrink them with a heat gun.

[1]

A cheap soldering iron + deburring tool

Why and how
A cheap TS100/Pinecil tip kit handles heat-set inserts, plastic welding and smoothing. Pair it with a swivelling deburring tool to trim elephant’s foot, tight holes and seams.

[1]

Slicer and infill

Infill is faster than walls.

Small part? 100% infill

On my Ender-3 V3 SE Good use for this printer: small, 100% infill parts like Multiboard bolts.

Do it in OrcaSlicer

Process settings, Strength tab. For one part only: right-click it in the Objects list, then Add settings › Strength.

  1. Walls › Wall loops 2
  2. Infill › Sparse infill density 100%
  3. Infill › Sparse infill pattern Rectilinear
  4. Infill › Internal solid infill pattern Rectilinear

Two walls keep the outside clean; the straight infill lines do the rest. Leave top and bottom shells as they are.

[6]

Why and how
Straight infill lines keep nozzle pressure steady and print faster than 6 to 10 perimeters. On small, thin or high-stress parts, 100% infill is faster, crisper and stronger than thick walls.

[1]at 30:10

What sticks to what

Pick a material to see its plate and prep.

MaterialBuild surfacePrep and release
PLAPEI spring steelWipe with fresh IPA from a wash bottle (never a spray bottle) and a paper towel before every print. [1]
PETGPEI spring steelNever use alcohol, it rips the PEI coating. Clean with brand-name Windex so its residue acts as a release agent. [1]
TPU / PEBAPEI spring steelTwo thick layers of glue stick, at right angles to each other. Dab warm water around the edges to swell and release. [1]
Engineering filamentsPEI spring steelMix Vision Miner Nano Polymer 50:50 with 90% IPA and apply 4 coats to a preheated plate. [1]
PCLTransparent inkjet labelsMust be transparent label sheets made for inkjet printers. [1]
Polypropylene (PP)Packing tapePP only sticks to itself, and clear packing tape is pure polypropylene. [1]
HIPSABS sheet or an ABS layerPrints cleaner on ABS than on Kapton tape. [1]
Nylon and PVDFUnclad FR4 or carbon fibre twillUnclad circuit board, carbon fibre twill or resin-soaked fibre plates tame warping. [1]
Acetal (Delrin)Heavy textured paperSticks to almost nothing else except thick, textured cardstock. [1]

Specialist filaments

Past PLA and PETG: plastics for toughness, bounce, chemicals and heat.

Key temperatures on one ruler

A ruler from 0 to 400 degrees C. 65 degrees: dry cardboard spools on the bed. 260 degrees: hardened steel nozzles lose their temper, and the Ender-3 V3 SE hotend tops out. Above 300 degrees: PPS-CF prints. 370 degrees: the QIDI Max4 hotend maximum.0100200300400 °C65°: dry spools260°: hardened steel limit · Ender max300°+: PPS-CF370°: QIDI max
Past 260 °C you need a tungsten carbide or gemstone-tipped nozzle. [1][2][4]

TPU (65D / GF-TPU)

Good at Practically indestructible layer bonds, shatterproof.

Catch TPU for AMS (65 Shore D) is golf-ball stiff. Siraya glass-filled TPU beats CF-TPU.

[1]

PCTG

Good at Tougher and clearer than PETG, and hydrophobic.

Catch Doesn't absorb moisture. Quirky until tuned, then reliable.

[1]

PEBA

Good at Real bouncy, rubbery rebound for bumpers and joints.

Catch Beats slow-recovering TPU whenever springiness is the goal.

[1]

Siraya Rebound Air

Good at Foaming PEBA. The lightest printable filament at its lowest density.

Catch Density changes with nozzle temperature, so it needs tuning.

[1]

PVDF

Good at Teflon cousin: low friction, crisp, chemical-proof, hydrophobic.

Safety Overheating releases formaldehyde and hydrofluoric acid.

[1]

PPS-CF

Good at Heat deflection above 200 °C, chemical-proof, rings like wrought iron.

Catch Prints above 300 °C (no enclosure needed) but is very brittle. Needs a carbide or gemstone nozzle.

[1]

SPS

Good at ABS-like and water-resistant. The clearest filament made.

Catch Don't confuse it with SEBS, a soft, floppy rubbery elastomer.

[1]

Infill finder

Every infill pattern has a job. What does your print need? [1]at 30:10

Rectilinear

Tiny gaps between alternating layers wick poured plaster or resin in by capillary action.

Aligned Rectilinear

Clear filament, smooth plate, 100% infill, +10 to 20 °C, slight overextrusion and 0 top/bottom layers gives glass-like clarity.

Grid

Fast default. Weak in tension, but the stacked crossings make it strong under Z compression.

Triangles

A non-skewing upgrade on Grid for fast-cooling PLA or soft TPU. Avoid on slow, brittle plastics.

Cubic

Even density in every direction, ideal for balanced dice, balls and rolling things.

Line

Lines that aren't parallel or at right angles make a 90s retro pattern inside clear prints.

Concentric

No overlaps and never anchors to the walls, so TPU and PEBA prints come out as soft and floppy as possible.

Honeycomb

No nozzle crossings and staggered double walls. The most forgiving for finicky filaments and clear prints.

3D Honeycomb

Minimal plastic-on-plastic contact. Very weak, but the gentlest pattern for ultra-finicky filaments.

Gyroid

Even strength in every direction (enough to turn walls off entirely), and hypnotic time-lapses.

Hilbert Curve

A fractal with no straight lines between opposite walls, which reduces warping in PEEK, PEI and nylon.

Archimedean Chords top/bottom

On top and bottom layers, gives a spun-metal finish on satin, silk or chameleon filaments.

Octagram Spiral top/bottom

On top and bottom layers with wood filament and wood stain, gives a handcrafted parquetry look.

Adaptive Cubic

Lowers density in the middle to save filament on bulky cosplay props.

Support Cubic

Puts density only under the top layers. Saves filament on tall, top-heavy busts and buildings.

Lightning

Texture hack: add 3 top layers, then a modifier 3 layers below the top with 0 top layers, 1 wall and 30 to 80% lightning, for a textured top skin.

Lateral Honeycomb / 2D Lattice

Sideways patterns that flex in one direction only, useful for watch bands.

Crosshatch

A faster, cooler-running alternative to Gyroid. A strong general-purpose default.

TPMS

Even strength like Gyroid but with no through-holes, ideal for closed-cell foams and waterproof squishy parts.

Cross Zag / Locked Zag

Cross Zag has a fish-scale look. Locked Zag sets separate edge and centre densities for batch production.

Zigzag / Quarter Cubic / Shark

Zigzag and Quarter Cubic have no clear practical edge. Shark is a legacy slicer Easter egg.

Takeaway: infill prints faster than walls. On small, thin or high-stress parts, 100% infill is faster, crisper and tougher than thick walls. [1]at 30:10

My printers

Main printer · since Nov 2026

QIDI Max4

Build volume
390 × 390 × 340 mm
Motion
CoreXY, enclosed
Hotend
up to 370 °C, 0.4 mm bi-metal nozzle
Bed
up to 120 °C, textured PEI
Chamber
heated, up to 65 °C
Firmware
Klipper + Fluidd
Extras
QIDI Box (4 spools, dries to 65 °C), Polar Cooler

Specs: [2][3]

Second printer

Ender-3 V3 SE

Build volume
220 × 220 × 250 mm
Motion
Bed slinger, open frame
Hotend
up to 260 °C, 0.4 mm brass nozzle
Bed
up to 100 °C, flexible spring steel plate
Firmware
Klipper + Fluidd

Specs: [4]

My settings

What I've measured on my own printers. A starting point, not gospel: your filament and printer will differ.

Ender-3 V3 SE · OrcaSlicer · 5 Nov 2026

eSUN PLA+ (Black, Matcha Green)

Nozzle
220 °C first layer, 215 °C after
Bed
60 °C, textured PEI
Pressure advance
0.04
Flow ratio
0.98
Layer height
0.2 mm (first layer 0.25 mm at 20 mm/s)
Drying
50 °C in the dryer, fed straight from it

Found with OrcaSlicer's pressure advance pattern test (0.01 to 0.10).

[5]

QIDI Max4 · QIDI Studio · 11 Nov 2026

Stock QIDI Studio profiles

Status
Using stock profiles while I learn the printer

Calibrated numbers go here as I measure them.

[5]

Sources

  1. 30 Hacks and Facts EVERY 3D Printer Should Know! Zack Freedman (Voidstar Lab), 11 November 2026 40m 21s. Main source for the tips, build surfaces, filaments and infill patterns.
  2. QIDI Max4 product page QIDI Tech Build volume, hotend, bed and chamber specs.
  3. QIDI Max4 FAQ QIDI Tech
  4. Ender-3 V3 SE product page Creality Build volume, hotend and bed specs.
  5. My own calibration prints and notes Jay Johnston Numbers I measured on my own printers. Your printer and filament will differ.
  6. OrcaSlicer wiki: Infill (Strength settings) OrcaSlicer Sparse infill density and pattern, and internal solid infill pattern.
  7. QIDI Max4 Extruder Clog Removal (Gear Version) Guide QIDI Tech, 3 February 2026 QIDI's official step-by-step video for clearing a jam in the Max4's gear extruder.
  8. QIDI Max4 Nozzle Replacement Guide QIDI Tech, 27 September 2026 QIDI's official video for swapping the Max4 nozzle.
  9. QIDI Max4 Maintenance Manual QIDI Tech Nozzle torque (1.5 to 2.0 N·m, tightened hot) and the heat-resistant gloves warning.
  10. QIDI Max4 wiki: Load filament QIDI Tech
  11. QIDI Max4 Hotend Replacement Guide QIDI Tech, 3 February 2026 QIDI's official video for swapping the Max4 hot end. No narration: the steps come from its on-screen captions.
  12. QIDI Max4 bimetal hot end (part page) QIDI Tech Fit the hot end with its cable clip facing outward.
  13. QIDI Max4 nozzle wiper, 5 pack (part page) QIDI Tech Spare nozzle wipers for when the old one is bent or cracked.
  14. Klipper G-Codes: PID_CALIBRATE Klipper Tune the heater after fitting a new hot end, then SAVE_CONFIG.

Updates

  • Extruder clog and hot end guides: added a numbered screw tray to the tools, so the screws from each step don't get mixed up.
  • Hot end guide: added my photo showing which two screws hold the hot end.
  • New step-by-step fix: replacing the Max4 hot end, from QIDI's video, plus my own checks so the nozzle wipe doesn't snap the new one.
  • New step-by-step fixes, each on its own page: clearing a clogged Max4 extruder and swapping the Max4 nozzle. QIDI's videos written out as tick-off steps, with a Show me clip for each step.
  • Site search (the magnifier at the top) now finds every tip, surface, filament, infill pattern and setting here, and everything is tagged with the other words people use, like garolite or cold pull.
  • Added the OrcaSlicer settings for the 100% infill tip.
  • Easier to scan: one-line tips with pictures, a Start here strip, a temperature ruler, and Listen buttons that read any section aloud.
  • Section started from my notes on Zack Freedman's 30 hacks video, plus my two printers and the PLA+ settings for the Ender.